Brand Name : Zhonggong Special Metallurgy
Model Number : GH132 Alloy
Place of Origin : China
MOQ : 100KG
Price : Price is negotiated based on the required specifications and quantity
Payment Terms : Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability : 5000 tons per month
Delivery Time : 5-8 working days, depending on the parameters required for negotiation
Packaging Details : Standard export packaging, or packaging as required
Name : Nickel Based Superalloy
Density : ~8.6 g/cm³ (0.310 lb/in³)
Melting Point : ~1300-1400°C (2370-2550°F)
Tensile Strength : ~950 MPa (138 ksi)
Yield Strength : ~750 MPa (109 ksi)
Elongation : ~15%
Thermal Conductivity : ~12 W/m·K (8.4 BTU·in/hr·ft²·°F)
Modulus of Elasticity : ~210 GPa (30 x 10³ ksi)
Corrosion Resistance : Good oxidation and corrosion resistance at high temperatures
Applications : Aerospace components, gas turbines, high-temperature structural parts
Certification : ISO Certificate
GH132 Alloy Is A High-Strength Nickel-Based Superalloy With Excellent High-Temperature Stability And Oxidation Resistanc
GH132 Alloy is a high-performance nickel-based superalloy designed for demanding high-temperature applications. It is known for its exceptional strength and stability under elevated temperatures, making it ideal for use in aerospace and industrial environments.
Key Properties and Features:
GH132 Alloy’s superior performance in extreme conditions ensures it is a trusted choice for advanced engineering applications requiring high durability and reliability.
Here is a composition table for GH132 Alloy:
Element | Composition Range (%) |
---|---|
Nickel (Ni) | 60.0 - 65.0 |
Chromium (Cr) | 14.0 - 16.0 |
Cobalt (Co) | 8.0 - 10.0 |
Molybdenum (Mo) | 2.5 - 4.0 |
Iron (Fe) | ≤ 6.0 |
Titanium (Ti) | 1.0 - 2.0 |
Aluminum (Al) | 1.0 - 2.0 |
Carbon (C) | ≤ 0.10 |
Manganese (Mn) | ≤ 0.5 |
Silicon (Si) | ≤ 0.5 |
Sulfur (S) | ≤ 0.01 |
These values are general guidelines. For specific applications or precise compositions, consult with industry standards or suppliers.
![]() |